My apologies to everyone who has asked me for a copy of the study our
manufacturingdepartment did on the Humiseal conformal coatings! I got
several requests for this study a couple of weeks ago & went in search of a
copy of the evaluation results. Much to my dismay I found that no report
was ever issued. And no one remembers the specific results except when they
thinned too much, the coating ran under the components without depositing a
thick enough film. The study specifically addressed brush coating or flow
coating under components. The work instruction was revised to reflect a
maximum thinning ratio of 10% by volume. Also, a thickness gauge was
purchased for use in ensuring that the average conformal coating on the
boards is maintained at 3 +/- 0.5 mils. So much for documentation, I
guess. Again, my apologies!!
Sheila Smith, Tracor Aerospace
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|