Hi Andy,
I can confirm that the 1 PPM Iodine had no effect on the many different
PWB products that we built during the timeframe we were using DI water
exclusively. I also believe that Chlorine might work also, but I cant confirm
that.
Regards,
Les Connally
[log in to unmask]
> From: Andy RJ McKean <[log in to unmask]>, on 8/14/97 9:47 AM:
> Hi L Connally
>
> Can you confirm that the use of iodine (even at 1PPM) will have no effect on
> product contamination.
>
> Regards
> Andy McKean
> [log in to unmask]
>
> -----Original Message-----
> From: mailnet
> Sent: Thursday, August 14, 1997 9:21 AM
> To: Andy R.J. McKean
> Subject: "Leslie O. Connally" <[log in to unmask]>: re:
> [TECHNET] Micro-organisms in rinses
>
> From: "Leslie O. Connally" <[log in to unmask]>
> Hi A. McKean,
>
> I'm not sure as to how to measure it, but about 1 PPM of Iodine in
> the
> water will kill most of the Microorganisms. We used this to kill algae in DI
> Water.
>
> Regards,
>
> Les Connally
> [log in to unmask]
>
> > From: Andy RJ McKean <[log in to unmask]>, on 8/14/97 9:05 AM:
> > Looking for info. on the effects and measurables of micro-organism growth
> in
> > rinse water. We have had a supplier mention this as a new problem
> occuring
> > in Europe.
> >
> > A. McKean
> >
> >
>
>
|
|
|