TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wm9Cf-000BjaC; Wed, 9 Jul 97 21:43 CDT
Old-Return-Path:
Date:
Wed, 9 Jul 1997 22:54:09 -0400 (EDT)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/13883
From [log in to unmask] Thu Jul 10 08:
50:29 1997
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"nc2Le3.0.a2K.Kn4np"@ipc>
>From willli Wed Jul 9 21:
43:49 1997
From:
X-Loop:
Message-ID:
Subject:
Parts/Attachments:
text/plain (47 lines)
In a message dated 97-07-09 05:27:25 EDT, you write:

>Having seen lots of SIR data from OTHER facilities, the problem could be a
>fault in the tester, or technique.  Did good old Bob retire around that
time?
> Did water quality in the rinse system change?  Did the DI water unit
>suddenly go south?  There are lots of factors that can cause poor SIR.
 Don't
>assume any one factor is the problem.  

Sir Doctor Guru of SIR

You run two pieces of laminate, one from vendor A, the other from vendor B,
through the same process, and one passes easily, the other fails miserably,
and you repeat this test, with 100% reproducability.... if you can make
another deduction from this data, TechNet is awaiting your assessment....:-)
>
>I do agree that no two laminates are the same.  Varying levels of porosity
>and varying resin compositions can dramatically effect SIR, or at least
their
>processing characteristics.
>
Sir Doctor:

Most of the poor, overstressed PCB fabricators have only their vendors to
(pick one) 1. turn to for assistance  2. blame, and having been in both
positions more than once, it is clear to me that we all need to see what the
options are.   I for one, and suspect many others, never considered that
laminate could vary to this extent.   This was a great learning experience
for me, and I was hoping to spread the benefits....

Yours in science, and PCB fabrication:

Rudy Sedlak
RD Chemical

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2