David,
Thanks for the tip. I should have looked there first before posting. Live
and learn. I looked over the last two years of archives and the drift of it
was that the white tin does not seem to have a whisker problem. However,
there were very few comments from people who had actually soldered boards
with it. Some negative comments appeared to relate to older processes than
the current commercial products.
Earl said he's seen some of these boards but worries about the tin surface.
Anybody care to share experiences with the current immersion white tin
products?
Regards,
Seth Goodman
Goodman & Associates
7687 Leta Way
Verona, WI 53593
Tel (608)833-9933
Fax (608)833-9966
> -----Original Message-----
> From: David D Hillman [mailto:[log in to unmask]]
> Sent: Thursday, January 07, 1999 8:49 AM
> To: [log in to unmask]
> Cc: [log in to unmask]
> Subject: Re: [TN] immersion white tin finish
>
>
>
>
> HI Seth - take a look back in the TechNet archives - it contains a couple
> of discussions on immersion tin and whisker phenomena.
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|