Yes, You can also plate with OSPs and Hard/TAB gold. This works very
well if you are utilizing Gold/Card Edge Connectors or something
similar that requires a gold contact surface.
Ni/Au PWBs in wave solder or SMT reflow solder very well. We limit
the Au thickness to 2-6 microinches (very important). We have
experienced some "peculiarities" in wave solder but not directly
attributed to Ni/Au PWBs. For some reason a Ni/Au PWB does not
tolerate touchup or post-wave assembly as well as a HASL or OSP PWB.
Maybe someone more knowledgeable on this topic can shed some
additional light.
Harlan
______________________________ Reply Separator
_________________________________
Subject: Selective PCB plating
Author: <[log in to unmask]> at INTERNET
Date: 3/10/97 9:49 AM
Does anyone know if you can selectively plate with OSPs and Immersion
gold on the same PCB? I would like to do immersion gold on my keypad
contacts but use something Like Entek on the rest of the PCB. Is this
possible?
My PCB assembly vendor doesn't like reflowing immersion gold PCBs. He
claims the solder doesn't flow very well. Is it just him or the rest of
the industry?
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************