TECHNET Archives

March 2015

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bob Wettermann <[log in to unmask]>
Date:
Mon, 30 Mar 2015 10:40:05 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Gumpert, Ben" <[log in to unmask]>
Message-ID:
Subject:
From:
"Gumpert, Ben" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Bob,

We both hand-tin and send parts out, and usually go with the hand tinning when it's small batches.
But we try not to tin any leadless components. Some packages probably wouldn't cause much problem, but QFNs can especially be trouble. The difference in size between the center pad and the pins means that you tend to get dissimilar volumes of solder on the tinned part, making them difficult to deal with at assembly. 

Ben

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Wettermann
Sent: Friday, March 27, 2015 9:29 AM
To: [log in to unmask]
Subject: EXTERNAL: [TN] Retinning to Meet JSTD-001 Guidelines for Gold Plated Parts

We have a contract where we have to place parts per JSTD-001 process guidance (Class 2 and Class 3).

There are some THOLE parts that are gold-plated (RF connectors) wit gold pins and some leadless SMT devices with gold pads.

Based on the client's interpretation of the spec all of these parts need to be tinned.

For such a small lot size (5 boards per P/N) are people hand tinning a few components or send them out to be retinned? What is your experience with the co-planarity of the leadless devices post tinning using a manual process?

Regards


--
Bob Wettermann
BEST Inc


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2