TECHNET Archives

November 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset=us-ascii
Sender:
Subject:
From:
"Roger M. Stoops" <[log in to unmask]>
Date:
Mon, 6 Nov 2000 09:09:50 -0500
MIME-Version:
1.0
X-To:
"Marsico, James" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (75 lines)
James,
What your vendor is proposing is the foil construction method of PWBs vs.
core construction.  For some vendors, foil construction saves a little
money, provides easier manufacturing (fewer innerlayer cores to process),
reduces warpage, and possibly a few other benefits one of the fab gurus
could comment on..  In the end you have the same, but possibly better,
board.  Most of our boards are foil construction, and we have seen no
problems with this form of PWB construction.
Roger M. Stoops, C.I.D., PCB Designer


Spectra Precision Inc./Trimble Navigation Ltd.
5475 Kellenburger Rd.
Dayton, OH 45424-1099 USA
Ph: 937.233.8921 or 937.233.4574 ext 288
Fax: 937.233.7511



                    "Marsico, James"
                    <James.Marsico@D        To:     [log in to unmask]
                    P.AIL.COM>              cc:
                    Sent by: TechNet        Subject:     [TN] MULTILAYER BOARD LAY-UP
                    <[log in to unmask]
                    >


                    11/06/00 08:21
                    AM
                    Please respond
                    to "TechNet
                    E-Mail Forum.";
                    Please respond
                    to "Marsico,
                    James"





Dear Techneters:

I have a six-layer board design which requires three polyimide cores bonded
together with two layers of prepreg.  Our PWB supplier is recommending
using
two cores bonded together with prepreg, then bonding copper foil on both
outside layers also using prepreg.  The resultant dielectric thickness'
would remain similar to the original design.  Are there any drawbacks to
this approach?  What is the benefit?

Thanks,
Jim M.

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2