Paymon,
Isn't this phosphor starvation what causes "black pad".

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paymon Sani
Sent: Wednesday, March 21, 2007 2:02 PM
To: [log in to unmask]
Subject: Re: [TN] Solderability problems on through holes only.

Hello Peter,

 

I have not looked at the suspect assemblies. However, this defect can
occur when the Nickel under the gold is oxidized prior to the TH
component assembly process. The electroless nickel is not pure and it
contains 10 to 14 percent phosphorus by weight. The nichel-phosphorus is
a good diffusion barrier to avoid corrosion of the solderable surface.
If the phosphor content is low i.e. 3 to 5% by weight then the
solderable surface will oxidize by each reflow heat application. The
oxidize nickel will then prevent soldering to the surface. The link
below is a good read on the ENIG surface finish.

 

http://www.pfonline.com/articles/129901.html

 

The assemblies should be reworkable with aggressive water soluble
fluxes, some mechanical action and a suitable soldering iron tip
temperature.

 

Hope this helps,

Paymon

 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Wong
Sent: March 21, 2007 4:18 PM
To: [log in to unmask]
Subject: [TN] Solderability problems on through holes only.

 

Hi Technetters,

 

 

 

We are having a solderability problem confined to only through hole

locations where we need some help or advice.  

 

 

 

We are soldering a no-clean SAC305 alloy to an ENIG finished board.  All

SMT solder joints (both sides) are fine.  During hand soldering in our

dedicated lead free area, we are having problems with solder wetting to

some of the annular rings and barrels of through hole locations, not all

holes.  The assembly is an 0.062" thick 4 layer 1"x1" board so it is not

thermally challenging.

 

 

 

We've built thousands of these in the past without this particular

problem.

 

 

 

The time lag between smt and through hole assembly is 1-2 days.

 

 

 

We've tried using a more aggressive flux such as OA flux with no

improvement.

 

The only way that we can get solder to wet is to mechanically scrape the

annular rings with a pick.  

 

 

 

Has anyone seen this before?  Why would this only occur on some of the

through hole locations and not on smt pads?

 

 

 

We have isolated this to a specific lot code of boards and are waiting

for some advice from our board vendor as well.

 

 

 

Thanks

 

Peter

 

 

 

 

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text
in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:
http://listserv.ipc.org/archives

Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815

-----------------------------------------------------


----------------------------------------------------------------------------
-----------
Confidentiality Notice

This e-mail and any attachment(s) are intended for the individual or entity
to which this email is addressed and may contain information that is
confidential.  If you are not the intended recipient or an employee or agent
responsible for delivering this e-mail to the intended recipient, please be
aware that any dissemination, distribution or copying of this communication
is strictly prohibited.  If you have received this in error, please notify
the sender by telephone at 604.430.4336 or by return e-mail, and please
delete or destroy all copies of this communication.  Thank you!

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2