TECHNET Archives

February 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 17 Feb 2012 18:42:37 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (63 lines)
Hi Jeff - fillet lifting is the result of the solder alloy solidification 
behavior. The tried and true Sn63Pb37 solder alloy the industry has used 
for year is a eutectic alloy - it changes from a molten state to a solid 
state at one specific temperature (183C). Many lead-free alloys, such as 
SAC305, are not eutectic alloys - they change from a molten state to a 
molten plus solid state (many folks call this the "mushy zone" to a solid 
state. Fillet lifting is associated with that alloy solidification 
behavior. It is easier to work with a metal alloy that has eutectic 
behavior as we avoid issues such as fillet lifting or shrinkage voids that 
are due to the alloy metallurgical reactions. Hope that helps.

Dave Hillman
Rockwell Collins
[log in to unmask]




Jeff Popp <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
02/17/2012 12:52 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Jeff Popp       <[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
[TN] Lead Free Fillet Lift






The IPC-610E, section 5.2.11 describes lead-free fillet lift as a 
"phenomenon in which the solder fillet is lifted off from the land on a 
board mainly during the flow solder process."

It sounds a little supernatural to me using the term "phenomenon."  I was 
just curious what exactly the cause(s) of fillet-lift were and why 
wouldn't it be considered a defect - similar to non-wetting?

Best Regards,
Jeff



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2