TECHNET Archives

September 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 11 Sep 2000 21:56:02 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Phil Zarrow <[log in to unmask]>
Parts/Attachments:
text/plain (42 lines)
Hi Kate (and all)-
I've written a number of articles about the ramp or tent profile and am
clearly and advocate of it.  It was made possible with the superior thermal
transfer capability and performance of modern convection dominant (forced
convection) reflow ovens.
In the past year, I did a project for one of the major data tracker
manufacturers where I characterized the parameters and specifications of the
major solder pastes on the market (it was for a self-profiling methodology
they the data tracker company was developing).  I queried all the major
solder paste manufacturers including AIM, Alpha, EFD, OMG, Kester, Indium,
Multicore, Senju, Qualitek, among others and included most alloys offered and
no-clean, RMA and OA flux formulations.  Over 90% of the formulations have no
problem at all with a ramp profile - i.e. no-soak.  It was put there many
years ago to accomodate the less efficient convection-IR oven methodology and
people came to believe the soak was required.
I am co-chairing (with Les Hymes) an IPC task group to re-define reflow
parameters.  A number of people Technetters would recognize (including Werner
E) are members of this group.  (Of course, being a comittee, my fear is that
by the time we hammer out a spec, reflow will be obsolete).  But in the
meantime, I urge everyone who has notg yet tried it, to do some experimenting
with the ramp profile.  It is not for every application, but it will work and
even improve most.
Regards,
Phil Zarrow
ITM, Inc.
Durham, NH  USA
www.ITM-SMT.com

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2