TECHNET Archives

February 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 15 Feb 2010 11:06:19 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Ioan Tempea <[log in to unmask]>
Parts/Attachments:
text/plain (57 lines)
Dear Technos,

 

I know the ImAg has been discussed over and over and with the same results, very good and reliable finish.

 

My little something now is all the proponents were mainly in high-rel applications (so SnPb solder most likely) and I do not remember if RoHS on Ag was discussed. I know it wouldn't make sense for this finish not to work with SAC305 pastes, but I just want to make sure.

 

 We have, guess what, wetting issues on two different boards, from the same supplier. We have tried playing with the reflow recipe, no improvement. The batch finished, but now we are attacking a few more different models 

from the same PCB fab.

 

So, did anybody have issues with ImAg because they were on lead-free? Any particular parameters that are not a happy ingredient, like specific types of paste, specific solder recipe milestones?

 

If it were the PCBs, what could be wrong except for the Ag thickness? I mean XRF analysis would be cheaper than x-sectioning...

 

Thanks,

 

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask] <mailto:[log in to unmask]>  
W | www.digico.cc <http://www.digico.cc/> 

 
 N'imprimer que si nécessaire - Print only if you must

 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2