Hi Inge:
Spray a scrap bare board that has not been cleaned and observe. Instead of spraying, brush some of the acrylic on a scrap board and observe. Take a sprayed board out of the environment to a warm room and let it dry there. Partial spray, partial brush and let the coating dry in a warm environment outside the normal environment. Order a new batch of coating and compare.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord
Sent: Tuesday, November 01, 2005 4:01 AM
To: [log in to unmask]
Subject: [TN] SV: [TN] Urgent! Acrylic coating
Hi all,
We have not solved the problem yet.
1. The Humiseal we use is 1B73
2. The thinner is 604
3. FTIR of 'crystals' gave VIGON 200 residues + poly ammoniumacrylate 4. No problems with nozzles or spray, no webbing 5. All mixing procedures according to Humiseal 6. Pattern does not appear until after some days 7. Pattern disappears after heat treatment of boards.
8. Humidity in air pipeline under investigation.
I'll send spectras to Steve FYI
Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Graham Naisbitt
Skickat: den 31 oktober 2005 13:22
Till: [log in to unmask]
Ämne: Re: [TN] Urgent! Acrylic coating
Hi Steve
WOW, I have never seen anything like that before. We shall study further and discuss with colleagues - weird.
Also, Dewey and I were both trying to get over to say "howdy" to you, but you had disappeared! We looked everywhere so have to figure you were out in the Casino?
--
Regards, Graham Naisbitt
[log in to unmask]
CONCOAT LIMITED
Alasan House, Albany Park
Camberley, Surrey GU16 7PH
Phone: +44 (0)1276 691100
Fax: +44 (0)1276 691227
www.concoat.co.uk
On 28/10/05 13:07, "Steve Gregory" <[log in to unmask]> wrote:
> Mornin' Inge!
>
> Well, I'm back from Vegas. Got out of there only $100 in the hole...I
> guess that's better than most people get out of there losing.
>
> Anyways, I have your pictures posted. Go to:
>
> http://www.stevezeva.homestead.com/files/Frosty_Pattern.jpg
> http://www.stevezeva.homestead.com/files/Frosty_Pattern_2.jpg
>
> That does look exactly like frost! Pretty weird!
>
> Kind regards,
>
> -Steve Gregory-
> Senior Process Engineer
> LaBarge Incorporated
> Tulsa, Oklahoma
> (918) 459-2285
> (918) 459-2350 FAX
> __________________________________________________________________
> This message may contain information that is privileged and
confidential to
> LaBarge, Inc. It is for use only by the individual or entity named
above.
> If you are not the intended recipient, you may not copy, use or
deliver
> this message to anyone. In such event, you should destroy the message
and
> kindly notify the sender by reply e-mail.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|