David Hillman <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, David Hillman <[log in to unmask]>
Date:
Fri, 21 Nov 2014 07:23:31 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (86 lines)
HI Juliano! The limits in the IPC JSTD 006 specification are for virgin
solder bar purchased from a solder alloy supplier and the limits in the IPC
JSTD 001 specification are for soldering processes - one column is for
preparation solder pots (pretinning, solderability testing, etc.) and one
is for assembly solder pots (wave, selective, etc.). You should be using
the IPC-JSTD-001 solder pot contamination limits.

Dave Hillman
Rockwell Collins
[log in to unmask]

On Thu, Nov 20, 2014 at 5:46 AM, Datacom - Juliano Ribeiro <
[log in to unmask]> wrote:

> Hi to all,
>
>
>
> We are analyzing my wave solder pot (contamination level).
>
> But we found in the IPC different limits.
>
> IPC-006B <>IPC-001C
>
>
>
>                 IPC06     IPC01
>
> Ag           0,1          0,1
>
> Al            0,005     0,006
>
> As           0,03        0,03
>
> Au          0,05        0,03
>
> Bi            0,1          0,25
>
> Cd           0,002     0,005
>
> Cu           0,08        0,3
>
> Fe           0,02        0,02
>
> Ni            0,01        0,01
>
> Zn           0,003     0,005
>
>
>
> In this case what is the correct to analyze my solder pot?
>
>
>
> Ps.: Alloy 63/37
>
> _____________________________
>
> Juliano Bettim Ribeiro
>
> DATACOM
>
> ENGENHARIA DE PROCESSOS
> Rua América Nº 1000 - Eldorado do Sul - RS CEP: 92990-000
> +55 (51) 8446-2135
>
> +55 (51) 3933-3000
>
> Ramal: 3484
>  <mailto:[log in to unmask]> [log in to unmask]
>  <http://www.datacom.ind.br/> www.datacom.ind.br
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________