I am trying to perform IPC-TM-650 2.4.44 Tack Test. The procedure calls
for a "Chatillon" tackiness tester or other equipment. I got some quotes
for tackiness tester, and they were in the neighborhood of $5000. It was
an Ametek tester. Does anyone have any alternative method/ equipment for
this test, or any place where I can purchase a used tackiness tester.
-Thanks,
Teo Tijerina
Conexant Systems, Inc.
915.780.5552
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|