Hi Vladimir,
For BP I am really only concerned about the surface, so EDS is fine--after
all it is the interface surface that is weak.
Cavitation (as a ME that word bothers me because cavitation is what a
propeller does in water) is a sign of the P notdoing its job.
So I stand by my definition.
Werner Engelmaier
Future workshops:
Solder Joint Reliability: Parts 1 through 4, July 17/18, Thal, Switzerland
Pb-Free Soldering Processes—Survival, Quality, Reliability, August 18,
Orlando
Reliability Issues with Lead-Free Soldering Processes, September 22,
Schaumburg
Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle Fracture,
ENIG), September 22, Schaumburg
**************
Gas prices getting you down? Search AOL Autos for
fuel-efficient used cars.
(http://autos.aol.com/used?ncid=aolaut00050000000007)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|