Can you put the mouse-bite breakaway on the edges of the boards next to the
throw-away tabs only instead of board to board? Would be easier than say,
having breakaway tabs on all four sides. 0.062" is common diameter for
single-pass routing operations (as well as 0.093" diameter). Also depends
on how the mouse-bite breakaway is designed (hole spacing. hole diameter,
holes in line with board edge, holes offset from centerline of board edge,
etc.
Rgds,
Roger M. Stoops, C.I.D., PCB Designer
[log in to unmask]
Trimble
Engineering and Construction Division
5475 Kellenburger Rd.
Dayton, OH 45424-1099 USA
Ph: +01 937.233.8921 or +01 937.233.4574 ext 288
Fax: +01 937.233.7511
Ken Patel
<[log in to unmask] To: [log in to unmask]
OM> cc:
Sent by: Subject: [TN] Spacing between board to board that has mouse/rat bite
TechNet design...
<[log in to unmask]
ORG>
11/12/01
01:03 PM
Please
respond to
"TechNet
E-Mail
Forum."
All,
My fab house is recommending 0.062" spacing between the boards on a
subpanel. I am using mouse-bite or rat-bite. As there are 5 boards per
subpanel, I would like to get opinion on the recommended spacing between
the boards and NOT between the board and throw away tabs. Here that
hangover needed to removed from both boards and if it's only 0.062" wide
then I believe it will be a bit little difficult to remove from the
second board once removed from the first board.
________________________
Board #1
________________________
this spacing
________________________
Board #2
________________________
and more....
Any suggestion will be highly appreciated.
Re,
Ken Patel
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|