Genny,

I continue to see black pad failures in this laboratory.  However, I
believe there is a kernel of truth in the statement that it is largely
understood and not as prominent as say 5 years ago.

Best regards,
Ed Hare, Ph.D.
VP SEM Lab, Inc.

---------------------------------------------------

               SEM Lab, Inc.
Scanning Electron Microscopy and Failure Analysis
               Snohomish, WA
           Ph. (425)335-4400
           Fax (603) 658-4519
           http://www.semlab.com
---------------------------------------------------



Genny Gibbard wrote:

>Just listened to a Lead Free presentation by one of our assembly materials
>suppliers.  They tested different pastes on different board finishes using a
>variety of different patterns, spacings, aperture sizes, etc,...
>By far and away, ENIG was the best finish for performance, for wetting,
>defects, voiding, ...
>The guy making the presentation said that he felt a lot of the initial
>concerns re ENIG - black pad being the biggest - have been resolved, and
>that they are no longer a concern, that they have determined what the cause
>of it is and eliminated it.  Anyone want to comment on that?  I'm not sure
>if he is correct, or just out of the loop.
>It was interesting as well:  ImmAg got a very bad rating from them in
>performance, even though many on this forum really praise that finish.  It
>exhibited dewetting (they printed solderpaste pads on an area with no
>soldermask, and the solder did not stay and spread where it was printed, it
>crept together with other pads into a big blob, like you might see a water
>drop do) and the amount of voiding was impressive!!
>About 4 years ago I joined this forum, and one of the reasons was because I
>was looking for info on ENIG.  We had done a prototype run of a couple of
>boards and they failed miserably.  They were never analyzed in depth, so it
>wasn't figured out what exactly caused the failure.  It was the excuse we
>needed to not choose this finish and some of the extra costs associated with
>it.
>However, with the Pbfree push now, I don't know if we should re-examine
>whether to use the finish.  For products where we needed a flat finish, we
>have gone to ImmSn, but we still use HASL wherever possible.
>
>Genny
>
>"Genius may have its limitations, but stupidity is not thus handicapped"
>Elbert Hubbard
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2