TECHNET Archives

September 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
multipart/alternative; boundary="-----------------------------1062729464"
Sender:
Subject:
From:
Date:
Thu, 4 Sep 2003 22:37:44 EDT
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (1209 bytes) , text/html (1859 bytes)
Steve,
   You are correct that acrylic and urethane have better resistance to
moisture and water vapor than silicone.  Silicone performs well in conditions of
complete submersion in liquid, however.  The main performance reason for choosing
silicone is high temperature operation, where silicone is superior.  For
chemical and acid resistance along with moisture, urethane is my choice.  For ease
of rework and moisture resistance, acrylic can't be beaten.

Jon Moore

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------


ATOM RSS1 RSS2