Multiply the diameter of one strand (in mils) by itself, and then multiply
the result by the total number of strands (CMA=D*DxN).
In your case, CMA=1.5*1.5*36 => 81
This is similar to a single strand of 31AWG solid wire.
Steve Sauer
Sr. Mfg Engineer
Northrop Grumman, Electronic Systems
Xetron
-----Original Message-----
From: Grabski III, John R. [mailto:[log in to unmask]]
This cable has 36 strands,
measuring 1.5 mils per strand. Can anyone help me with a URL or a makeshift
chart including smaller wire gauges?
Much appreciated.
-John Grabski III
Badger Technologies Inc.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|