If the nickel is on the copper trace under the covercoat in a bend area you
are in trouble. Steve Kelly
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Jindra, Larry
Sent: Thursday, May 24, 2001 3:16 PM
To: [log in to unmask]
Subject: [TN] ENIG in flex layers
Our rigid/flex vendor deposited immersion gold over electroless nickel on
internal 1 oz copper flex layers prior to lamination of a rigid-flex-rigid
board. Our intent was to have ENIG finish only on the exposed connector
pads on the one end of the rigid/flex (6 layers). Instead, the ENIG is on
the pads, on the flex, and continues on in internal to the other rigid
portion of the circuit board (10 layers).
I have concerns about the durability of the flex and the via stackup in the
10 layer rigid section, which now has nickel on layers 3 & 8. Am I just
paranoid, or am I in trouble?
> Larry Jindra
> mailto:[log in to unmask] ph (858) 592-3424 fax (858) 592-3940
>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|