TECHNET Archives

July 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 1 Jul 2011 08:34:14 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Message-ID:
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (155 lines)
Thulium

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Friday, July 01, 2011 7:08 AM
To: [log in to unmask]
Subject: [TN] NTC Friday Element Quiz - the Question

Hi folks - Here is the Friday Element Quiz Question:

The Question:

This element is used for research purposes only. There are no commercial 
outlets for the element as Sodium can be used to accomplish the same tasks 
at a much lower cost. This element is more expensive than gold or platinum 
(*** per my reference source). A pure sample of this element was not 
produced until 1928. Apples contain 50 ppm of this element but plays has 
no known biological role.

Bonus Question: Name the mineral that contains this element.



The quiz winner will get to put Clumpy and Kloumpios to work for them for 
the week.

So far Clumpy and Kloumpios have:

Week 1 Lamar Young, SCS Coatings
- accomplished nothing (drank lots of coffee)

Week 2 Bev Christian, RIM
- conducted REACH material testing

Week 3 Drew Meyer, Benchmark Electronics Inc.
- Solderability testing and mowed the lawn

Week 4 Ian Fox, Goodrich
- had an epic journey of travel

Week 4 Gary Ferrari, Garrick Global
- unknown

Week 5 Fredrick Miller, Astrolab
- unknown

Week 6 David Nelson, Raytheon
- Were tackling dummys for Dallas Cowboys

Week 7 Graham Collins, L3 Communications
- Cleaned gutters and painted window trim

Week 8 Bill Noel, ITT Geospatial Systems Division
- unknown

Week 9 Steve Gregory of RD Circuits
- unknown

Week 10 David Bealer of Watchfire Signs
- descaled the in-line wash machine! Ouch!

Week 11 Dick Krug of Sparton Corporation
- assisted with AS9100 quality management systems requirements audit

Week 12 Steve Creswick of Balanced Enterprise Solutions
- Acted as Steve's "go fer" due to a broken leg!

Week 13 Gebhard Neifer, Delphi
- conducted a plasma pre treatment Taguchi DOE for a sealing process

Week 14 Bev Christian, RIM
- assisted with a tin pest investigation/test

Week 15 Bev Christian, RIM
 - assisted Bev shoveling snow

Week 16 David Bealer of Waatchfire Signs
 - assisted with reflow profiling

Week 17 Brian Ellis, rumored to be retired
 - assisted with rewiring the house, had a tractor accident and found
his cousin Kloumpios

Week 18 Denny Fritz, SAIC
 - assisted with tin whisker inspection/examinations

Week 19 Graham Collins, L3 Communications
- assisted with scraping barnacles, boat paint and boat engine
maintenance

Week 20 Mark Woolley, PTRL Laboratory Avaya
- assisted with weather observations (70F to snow) and resolving 
electrochemical migration failures

Week 20 Tom Carroll, Boeing Defense, Space and Security
- assisted with commercial aircraft galley inspection

Week 21 Brian Ellis, supposedly retired, and Tom Carroll, Boeing Defense, 
Space and Security
- assisted with root cause corrective action tasks
- assisted with nothing but catching up with the family

Week 22 Drew Meyer, Benchmark Electronics Inc.
- assisted with metallographic cross-sections and Dye & Pry testing

Week 23 Bev Christian, RIM
- assisted with a creep corrosion project and the setting up of an oxygen 
bomb

Week 24 Steve Gregory, RD Circuits
- assisted with ?????

Week 25 Ahne Oosterhof, A-Laser
- assisted with stencil aperture data analysis and split/stacked firewood

Week 26 Scott Post, Delphi
- assisted with ????

Week 27 
- assisted with ????

Dave Hillman
Rockwell Collins
[log in to unmask]

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2