TECHNET Archives

November 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
X-To:
Date:
Tue, 13 Nov 2012 16:19:12 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Amol Kane <[log in to unmask]>
Subject:
From:
Amol Kane <[log in to unmask]>
Message-ID:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Sender:
Parts/Attachments:
text/plain (29 lines)
Hi all,
Resending the original e-mail as plain text because I don't think the original went thru. Please disregard and my apologies if you receive a duplicate.


We have this unusual (at least for me) request from a potential new customer. This is taken verbatim from their request for process information. Before I go and tell them this cannot be done, I want to ask the experts out on technet if they have seen/done something like this. My thinking is that this would be very hard to do on the floor unless there is a custom formulation available. I am not aware of their reasoning for asking this other than for a very unusual (and ineffective) way of mitigating tin whiskers. Leaving the potential flux incompatibilities aside, is this something that is being done/can be done? I could use some expertise or references/studies on # 2 as well.

1.      "Since our products are not subject to RoHS and our customer is not requiring lead mitigation, is there a vendor preferred process of Pb based or Pb-free processing.
a.      Describe your history/experience and process for adding ~3% Pb to Pb-free paste and utilizing Pb-free processes.
b.      Any quality or reliability concerns adding ~3% Pb to Pb-free soldering.
c.      Describe your history/experience and processes used in transitioning a product from Pb to Pb-free (or reduced Pb).
2.      Do you know of any issues with RoHS and reliability at -65C?"

Thanks,
Amol



________________________________
Confidentiality Notice

This e-mail and any attachment(s) are intended for the individual or entity to which this email is addressed and may contain information that is confidential. If you are not the intended recipient or an employee or agent responsible for delivering this e-mail to the intended recipient, please be aware that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this in error, please notify the sender by telephone at 604.430.4336 or by return e-mail, and please delete or destroy all copies of this communication. Thank you!

P     Please consider the impact on the environment before printing this email or its attachments

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2