TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 7 Jul 2010 19:19:32 +0200
Reply-To:
Subject:
From:
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
MIME-Version:
1.0
Parts/Attachments:
text/plain (88 lines)
prepare a professional report (NASA, Lockheed Martin, Oreal, ESTEC, Boeing
etc customers) with all arguments for a better way of MMIC mounting.  Full
list of references and stds.  Will see if I can involve you.  Sending
pictures offline to you.
/Inge

--------------------------------------------------
From: "Steven Creswick" <[log in to unmask]>
Sent: den 7 July 2010 17:14
To: <[log in to unmask]>
Subject: Re: [TN] Hybrid precap q

> Inge,
>
> I would cut back on the adhesive deposited and dictate less than or equal
> to
> 50% climb up the side of the device.
>
> They can verify bond strength and coverage by die shear.  They could also
> verify coverage by cutting thin glass plate to the size of the devices and
> inspecting after placement.
>
> I agree with your concern.
>
> Can I get part of your fee??  .... I work for fuel costs....   :-)
>
> Steve C
>
>
> On Wed, Jul 7, 2010 at 6:16 AM, Inge <[log in to unmask]> wrote:
>
>> Hi  all,
>> will be back with quiz 11, but before that , I have a q about silver
>> epoxy
>> mounting MMIC chips.  The amount of glue is so rich, that the silver
>> epoxy
>> wets all the way up the walls and stops just before the horizontal plane
>> of
>> the chip. Now, some conductors are as close to the chip edge as two times
>> the diameter of a bond wire, which is about 50 um. I dislike such a small
>> distance between the silver and the conductors.  I'm doing a consulting
>> job
>> for a company, and they mean  that this space is enough. The chips are in
>> a
>> laserwelded kovar package, so they are well protected, but I'm still not
>> satisfied. I've seen too much of migration issues in my days.  The
>> packages
>> are class S. What are your opinions?
>> Thanks in advance
>> /Inge
>>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2