TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Cash, Alan" <[log in to unmask]>
Date:
Fri, 17 Jul 1998 10:07:45 -0400
MIME-Version:
1.0
X-To:
Neil Atkinson <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Cash, Alan" <[log in to unmask]>
Parts/Attachments:
text/plain (44 lines)
 I "suspect" that you "might" have a problem with solderability.  How soon
after manufacture of the switch do you assemble and solder into the PCB?
You have a problem with brass pins that have no barrier plating.  The zinc
from the brass will cause soldering problems.  The silver may slso cause a
problem but I have had no experience with that type of silver.  Maybe
someone else on the net has soldered to that plating.

      Al Cash.

> ----------
> From:         Neil Atkinson[SMTP:[log in to unmask]]
> Reply To:     TechNet E-Mail Forum.;Neil Atkinson
> Sent:         Friday, July 17, 1998 9:03 AM
> To:   [log in to unmask]
> Subject:      Soldering microswitch legs
>
> Technetters,
>
> I am currently having problems soldering a switch to A PCB.  I have asked
> the manufacturer what the switch terminals are made of and he has come
> back with the following:
>
> One lead is CuZn37 (Brass) plated with 12 microns of electrolytic gold.
>
> Whilst the other lead is the same base with 2 microns of hard bright
> silver argilion passivation and 2 microns gold.
>
> Can anyone tell me the implications of wave soldering this to a PCB?
>
> Neil Atkinson
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################