     To aid in fiducial recognition a different surface finish will help 
     such as OSP or Electroless Ni Immersion Au.  Another alternative would 
     be a clear soldermask over the fiducial.  This would require the 
     entire board to be clear mask and assumes this product is mask over 
     bare copper (SMOBC).  This type of change could be less traumatic to 
     the assembly process than changing surface finish.
     
     Guy Willingham
     Zycon, A Business Unit of Hadco Corp.
     [log in to unmask]

______________________________ Reply Separator _________________________________
Subject: FIDUCIALS
Author:  [log in to unmask] at corp
Date:    3/9/97 11:48 PM


Hello Technetters,
     
I am having a slight problem with the amount of solder on fiducials. This is 
causing optical recognition problems during the pick and place.
     
Any suggestions, maybe an alternative surface finish.
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2