the silence is deafening. Guess I'll chime in.
At 06:02 AM 11/10/2010, Post, Scott E wrote:
>I'm curious what people are using for 0.4 mm pitch BGAs:
>
> - Copper pad diameter
250um is typical
> - Soldermask or non-soldermask defined?
yes. >:-}
> If NSMD, what size soldermask opening?
Depends on uVia technology used.
1. Standard copper via in pad: 250um w/ 300um pad
2. ALIVH compromise:
•Via pad size enlarged to 300um
•S/M opening enlarged to 400um.
•S/M dam of 100um width added
• Accept Potential S/M encroachment one side of pad
> - Paste stencil thickness and aperture size (round or square?)
fielders choice? :-)
>I'm playing with different designs and it's
>quite a balancing act between pad size, board
>suppliers' soldermask registration tolerances,
>and having pads large enough for suppliers' via
>in pad design guidelines. One option is to get
>rid of soldermask completely from under the part
>since, except for the outer row, there's no room
>for trace routing on the outer layer anyway.
>
>Scott Post
>Staff Manufacturing Engineer
>P.O.U. 0000-001E-0CTC
>2151 E. Lincoln Road
>Kokomo, Indiana 46904-9005
>765-451-2983 (Phone)
>765-451-0287 (FAX)
>
>****************************************************************************************
>
>Note: If the reader of this message is not the
>intended recipient, or an employee or agent
>responsible for delivering this message to the
>intended recipient, you are hereby notified that
>any dissemination, distribution or copying of
>this communication is strictly prohibited. If
>you have received this communication in error,
>please notify us immediately by replying to the
>message and deleting it from your computer. Thank you.
>
>****************************************************************************************
>
>______________________________________________________________________
>This email has been scanned by the MessageLabs Email Security System.
>For more information please contact helpdesk at x2960 or [log in to unmask]
>______________________________________________________________________
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of
>Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts:
>send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach
>Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|