This is for "research". We are fabricating micro coils on silicon and glass
wafers. Basically, evaporate gold, then spin-on PDMS (photoresist), then
pattern it - say, 100micron long 10 micron wide trenches. And then plate
these trenches with (trying different materials. maybe will be something
else in the end):
1. copper
2. nickel
3. cobalt
4. cobalt alloys
these are all 2" wafers - will never go bigger than that.
Adhesion is important. if you ask me, very important. but not necessarily at
this stage. right now I am just trying to understand what the heck am I
doing :-)
Lifetime? Few days will do it for now. Theoretically, in the end I will coat
whatever I will make with Teflon so lifetime will be as good as adhesion.
Thanks a million.
By the way, right now I'm talking to TekNu for a wave-sequencing power
supply, Atotech for chemicals (acid-copper plating solution for now), and
I'll make my plating cell out of a 100ml beaker. Does that make sense?
I'm looking for a link of the type "electroplating for dummies" or "learn
how to electroplate in 15 minutes" :-) I have a test power supply that will
be in my hands in exactly 2 weeks and I need to have everything ready by
then. I need to have some (but little is enough) understanding what I am
doing.
Thank you very much!!!
------------------
Greg Fridman
School of Biomedical Engineering, Science & Health Systems
BioApplications Group, Drexel Plasma Institute, Drexel University
Office: 215-895-0576 Cell: 312-371-7947 Home: 215-387-3161
AIM: zegogga MSN: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: Thursday, October 23, 2003 4:15 PM
To: [log in to unmask]
Subject: Re: [TN] electroplating newbie
Hello Gregory,
There are a number of potential solutions but you need to answer a few
questions before a good answer can be arrived at.
How big is your part? What is/are the material(s) you wish to plate? How
thick? How important is adhesion? What is the use environment? What lifetime
do you expect?
Kind regards,
Joe
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|