Every six months, we check:
Tip temperature variation +/- 5C
Tip-to-ground resistance 2 ohms max.
Tip-to-ground potential 2 millivolts max.
These tests are based on an old mil spec, and while they
are a little more stringent than J-1, our irons
meet these limits, so we haven't seen the need to change.
-Joe
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jeff Popp
Sent: Tuesday, July 28, 2009 9:30 AM
To: [log in to unmask]
Subject: [TN] Soldering Iron Verification
We are attempting to establish a calibration/verification schedule for our hand-held soldering stations as recommended in the J-STD-001, Appendix B.
It states that frequency should be in line with manufacturer's recommendations.
I was curious if anyone else has a calibration/verification schedule established for their soldering irons, and if so, what frequency? What other controls, if any, do you apply?
Best Regards,
Jeff
Jeff Popp
Quality Assurance Technician
Compunetix
2420 Mosside Blvd.
Monroeville, PA 15146
(412) 858-6184
[cid:[log in to unmask]]
"Difficulty is the excuse history never accepts." ~ Edward R Murrow
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|