TECHNET Archives

August 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 11 Aug 2003 13:57:29 -0700
Reply-To:
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Eddie Rocha <[log in to unmask]>
In-Reply-To:
Content-transfer-encoding:
7BIT
MIME-Version:
1.0
Parts/Attachments:
text/plain (20 lines)
I have a similar question. Not black pad rework but rework on SMT
pads (actually the entire PCB exposed surface) which were coated with
White Tin. I can't seem to get the tin stripped to recoat it with tin. The
PCB's are almost 1 yr old and I'd like to recoat with fresh tin. I did this
successfully with a number of different part numbers. But I have this
one set of boards that I can't get it back to a clean bare copper
surface. Does anybody have suggestions?  More ggressive
microetching didn't work.

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2