Hello Seppo,
Underfill will definitely "save" you from having cracked joints (particularly due to drops), but it's a "painful" procedure.
Regards,
Vladimir
Vladimir Igoshev
Research in Motion
-----Original Message-----
From: Seppo Saario [mailto:[log in to unmask]]
Sent: Thursday, December 18, 2003 8:49 PM
To: [log in to unmask]
Subject: [TN] BGA Underfill comments/recommendations
Dear All,
I am doing some checking into the effectiveness of BGA underfill on mobile
handsets.
Typically handset boards have 3-4 BGA's (0.5 to 0.8mm pitch) and have seen
handsets with and without underfill.
PCB thickness is 0.8mm
Has anyone seen any studies, or have any comments on the reliability of BGA
joints wrt underfill.
Also, any comments on what typically recommended underfill compounds are is
also appreciated.
Thanks in advance! - and wishing you all a Merry Christmas and a Happy New
Year !.
--
Seppo Saario
Voxson Ltd., Core Technologies - Hardware
Design Engineer
Tel +61-7-3268-0745 ; Fax +61-7-3878-1370
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Friday, 19 December 2003 10:20 AM
To: [log in to unmask]
Subject: Re: [TN] Need your opinion
I would agree with the shearing rather than routing of the edges. With the
severe crazing that extends to the ball area, it is a realiability issue.
The cracking of the solder mask is a real concern and indication that the
edges are suspect.
Susan Mansilla
Robisan Lab
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
Main Switch: +61 7 3868 1277 Fax: +61 7 3868 1370 Home Page:
www.voxson.com
Local Time : GMT + 10 hours
Disclaimer - This e-mail is intended only for the addressee(s) named
above. This e-mail may contain confidential or privileged information.
No confidentiality or privilege is waived or lost by any
mis-transmission. If you are not a named addressee, or the person
responsible for delivering the message to the named addressee, please
telephone the sender immediately on the number above and delete the
message. You must not disclose, copy or rely on any part of this
correspondence if you are not the intended recipient.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|