TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 1 Nov 2005 15:53:47 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Genny Gibbard <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Genny Gibbard <[log in to unmask]>
Parts/Attachments:
text/plain (47 lines)
The general consensus that I am hearing these days is that Bi in the
1-4% range is acceptable.  Otherwise it could be a problem.
We use an NEC part as well (single sourced), and have already had to
deal with confirming this. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Barr
Sent: 1-Nov-05 3:33 PM
To: [log in to unmask]
Subject: [TN] SnBi Lead Plating

We received a last time buy notice from a distributor for a NEC part.
The part is going to a RoHS compliant finish. The information we
received seems to indicate the lead finish will be SnBi. With the
transition from Pb to Pb-free still happening, it seems like a problem
to have Bi on a component lead. Everything I have read says Bi cannot be
mixed with Pb because it forms a low temperature melting alloy. Has
anybody heard of Bi being used in a component lead finish? I'm hoping
this may just be a mis- communication.

Thanks.

Bob

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2