Hi Johannes,
There is some debate about Solder Mask Defined (SMD) pads for BGAs. Some
papers indicate that Non Solder Mask Defined (NSMD) pads increase the fatigue
life of the solder joint (SMD pads cause stress concentration point in solder
joint). However, it is interesting to note that many of the BGA component
suppliers actually use SMD pads on the BGA substrate. So, although you can
choose SMD vs NSMD for your board, the supplier dictates the substrate design
(typically SMD).
To address your overprinting question (printing paste on solder mask), we have
been using overprinting for Ceramic BGAs successfully for the past couple of
years without problems. The paste will pull back to the solder joint. You
may want to verify on your particular assembly (X-sections, etc.).
Hope this helps.
Charles Elliott
Newbridge Networks
--------------------------------------
The pads of PBGA`s that we use are defined by solder mask on our
multilayer FR4 pcb`s
The diameter of stensil aperture is bigger than the pad diameter , so we
are actually printing
( no-clean ) paste on the soldermask.
Is this OK, or should it be avoided ? I presume that the adhesion between
stensil
aperture-paste is bigger than the other one between soldermask and paste,
resulting
to increased risk to solder balls, which could be fatal under PBGA ( pitch
.05" )
Stencil width is 0.15 mm ( 6 Mils ), laser cut
Stensil diameter .56 mm ( 0.22" )
Pad diameter 0.72 mm ( 0.28" ) max
Solder Mask diameter 0.52 mm ( 0.20" )
Any opinions?
Brs, Johannes
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|