TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Pratap Singh <[log in to unmask]>
Reply To:
Date:
Fri, 07 Mar 1997 09:05:55 -0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (45 lines)
Sheila Smith wrote:
> 
> Technetters:
> 
> I am soliciting opinions on conformal coating of PBW-mounted connectors.
> Our manufacturing folks refuse to conformal coat within 1/8" of any board
> mount connectors.  They contend the conformal coating will wick up the pins
> and get on the contact areas, regardless of the type of conformal coating
> used or the method of application.  The connectors are not sealed.  These
> boards have to pass salt fog & humidity testing and I don't like the idea of
> having bare areas, especially at the interface where the connector meets the
> board.  Does anyone have any experience with this?  Thanks in advance for
> your help!
> 
> S. Smith, Tracor Aerospace Electronics Systems
> 
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
> * with <subject: subscribe/unsubscribe> and no text in the body.          *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact   *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
> ***************************************************************************
Sheila,  there are ways to protect the connectors while the boards are
being coated with a conformalcoating. You can tape them individually or
design a cover fixture if they are adjacent to each other.

It all depends upon how the boards are being coated? by spray, dipping
or a vapor deposition method like used for "Parylene" conformal coating.


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2