Michelle,
there are ways, some of which have to be performed when all have gone home.
All depends on what components you point at.
If it is a bad nickel you can test ultrasonic solder dip, use to fix most
problems without causing damage to the parts.
If it is a bad nickel/exposed copper I recommend use of RA soldering.
If it is a bad nickel/exposed Kovar you can normally get a acceptable
soldering by dipping the leads in Zinc Chloride one minute or two.
The last one deseves a warning, because you need a real good cleaning
afterwards. Furthermore, the component can be damaged. And your QA will kill
you.
Finally, you can strip the leads and dip the leads in chemical
nickel/chemical gold baths. Expensive and time consuming,but if you have to
do with extremly expensive components or obsolete parts, it can be a way to
solve the problem.
You need a old chemo dog with stick and thick glasses to do the last one.
Inge
----- Original Message -----
From: "Michelle Masaitis" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, November 18, 2010 4:41 PM
Subject: [TN] Old obsolete parts failing test
Does anyone have any recommendations on parts that are more than 5 years
old for getting them to solder. You can see that parts reflow around the
lead,
but when you take the part off of the pads there is no solder on the bottom
of the lead. These parts fail test, but then we add stronger flux and use
hot
air to re reflow and the part passes. The leads are not bent, they are
flush to
the board. We changed solder paste, which did help some, but not
completely. I would like to use the parts without having to send them out
to
get the leads tinned before placement. These parts are obsolete so they are
hard to find parts. Any recommendations? Thanks for your input.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|