Bob
I suggest, as it's an acrylic and easy to strip, you strip the lot, do
your rework, clean and recoat. It's risk-free. A pure water wash at < 60
°C will probably not do much harm to an acrylic but any temp excursion
(wash or dry) > 70 °C will certainly damage it. Any additive to the
water ditto. Play safe.
Brian
bbarr wrote:
>
> I have some boards that are coated with acrylic conformal coating. We have
> to do a few chip replacements. The coating will be selectively stripped
> around the chips and the rework performed. Is there a problem with sending a
> coated board through an in-line aqueous cleaner? I am running just water at
> 130 degrees F. Will the pressure damage the coating? Will the water
> recycling system become contaminated? Do I have to strip the board
> completely prior to rework to avoid any problems?
>
> Thanks for your help.
>
> Bob
>
> Robert Barr
> Manufacturing Engineering
> Formation, Inc.
> Voice: 856-234-5020 x3035
> Fax: 856-234-6679
> email: [log in to unmask]
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|