TECHNET Archives

August 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Paul Edwards <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Edwards <[log in to unmask]>
Date:
Tue, 28 Aug 2007 12:16:47 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (82 lines)
Tim,

Try cranking up the heat on your Pb-free soldering iron and gently
rubbing the solder mask from the area on top of the Cu pads... The
solder mask adhesion to the Cu as well as the solder mask should start
breaking down...  Be careful because the heat will also cause the
adhesive holding the Cu pad to the laminate to weaken...Once you get the
hang of it you can do this all day.... We sometimes have to... Oh, say
good bye to the tip or designate it your "solder mask scrapping" tip

Paul 

Paul Edwards
Process/Quality Engineering
[log in to unmask]
Tel: 408-433-4700
FAX: 408-433-9988
Surface Art Engineering
81Bonaventura Dr.
San Jose, CA 95134
DUNS: 944740570
CAGE/NCAGE: 1XZ48

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tim Mack
Sent: Tuesday, August 28, 2007 11:25 AM
To: [log in to unmask]
Subject: [TN] Solder Mask Solvent?

All,

 

I have run into an issue with a board that has solder mask covering some
pads.  Is there a product/solvent that can remove the solder mask easily
with out etching the copper?  I would rather chemically remove it than
manually scrap it off with a razor blade.

 

Thanks in advance,

 

Tim Mack

Research Engineer

NDSU CNSE

www.ndsu.edu/cnse

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2