Just a thought. Has anyone tried correlating flux ionic readings with
activity levels?
It would be interesting to use flux until it almost stops soldering
while continuously monitoring ionic readings of a fixed volume of the
flux. Maybe some accept/reject indicator could be obtained.
Jim Kittel
>-----Original Message-----
>From: [log in to unmask] [SMTP:[log in to unmask]]
>Sent: Tuesday, December 01, 1998 7:30 AM
>To: [log in to unmask]
>Subject: [TN] Flux activity monitoring system
>
>I'm sure you know this, but checking flux specific gravity (in accordance
>with supplier requirements
>at a specified temperature) with a calibrated hygrometer is best. Worst, is
>using so called
>automatic systems that are part of some wave solder machines. Also, don't
>keep replenishing or
>"thinning" flux. It's cheap, compared to defective solder joints, so dump and
>replace regularly
>(when sg starts falling off say at the end of a shift or production run).
>Hope I didn't over-
>simplify, but it's all I know.
>
>Earl Moon
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
>for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|