TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 4 Nov 2004 13:46:31 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Lee Parker <[log in to unmask]>
Subject:
From:
Lee Parker <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (138 lines)
Steve and All

I installed the first immersion silver line in North America at the AT&T
facility in Richmond, VA. We began the evaluations in 95. Initially,
Lucent was the only customer, but in time many more followed. I was
never disappointed in its reliability or performance.

I am sure George Wenger or Bob Furrow can discuss the results at the
Lucent assembly sites and the reliability work carried out prior to
using the product.

Best regards

Lee


----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Precision Lab
Sent: Thursday, November 04, 2004 1:02 PM
To: [log in to unmask]
Subject: Re: [TN] PWB Immersion Silver Finish

Hello Victor,

I hope you do not mind me responding to this message sent to Steve.
Steve
I also hope that you do not mind as well.  However, we have just
completed
a study for a company that was using immersion silver (IAg) surface
finish
along with lead-free pastes. As part of our study we did some heavy
research into the IAg process and its benefits and pitfalls, as it were.
Here is what we found as a result of our research:

Advantages of IAg:

* Cost, the cost is comaparble to HASL.
* The surface after application is flat, unlike that of HASL.
* IAg produces better signal integrity, especially in higher frequency
applications.
* Applied silver by electroless application doesn't require high
temperature excursions or exposure to unpleasant chemistries.  It is a
very simple process.
* Shelf life of IAg boards is approxiamately one year, this is
comparable
to HASL.
* Lastly, the IAg surface finish has 100% wettability and is not prone
to
discoloration.

Disadvantage:
* Silver nitrate used in the application process is very light
sensitive,
thus the immersion bath should be enclosed.

In the past IAg surface finish had issues with electromigration
(dendrites), this is now an urban myth.  IAg has progressed to the point
that it is no longer at any more of a risk than any other surface finish
for electromigration.

We were able to derive alot of information about IAg from Don Cullen of
MacDermid and our research fell in line with what he told us. He was
gracious enough to talk at length with us about this particular finish.
I
would imagine he would also speak with you or whoever.  Should you
desire
to speak with him, his phone number is (203) 575-5658.

As far as what we have seen with LF pastes at this point, it appears to
work well, at least for the pastes that we have tested.

I hope this helps!

Best Regards

Joe Russeau
Process Analyst

Precision Analytical Laboratory



Steve,
>
>    Can you share your experience with PWB Immersion Silver Finish?
> ie.   shelf life, usage after package is opened, storage of non
process
> PWB, surface oxidation, compatibility with LF solder.
>
> Victor,
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
[log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2