TECHNET Archives

September 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 9 Sep 2008 16:50:43 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, fabrice pires <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Subject:
From:
fabrice pires <[log in to unmask]>
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
In-Reply-To:
<976C1AE0F27B4DF4A90CD25C78E0577D@ingemar2a39615>
Organization:
Thales-EPM
MIME-Version:
1.0
Parts/Attachments:
text/plain (23 lines)
Hi Techneters,

I would like your advices on the best way to calibrate XRay pictures in 
aim to measure precisely voids inside BGA balls, after assembly.
Everyone should agree on the fact slight setup variation on XR equipment 
could change significantly the void size results.

Do you have any trick to improve precision measures whatever the XR 
equipment?
Does the use of any reference/calibration on boards exists in that aim?

Fabrice

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2