A considerable amount of information has been given in this forum about "Pink
Rink" and its effects in the PC Board process.
As an OEM of assembled boards, I would like to know what the effects of this
condition are at the functional level; and is there any way to identify Pink
Ring at the finished bare-board or assembled/soldered level.
Thanks in advance,
Bill Watson