Have the smallest PTH on the board also in the test coupon.
Have test coupon in different areas of the panel, if this is possible.
Make an electrical test on the bare boards (but will only detect open circuit).
Best Regards
Peter Dahlén
Saab Ericsson Space
At 16:11 1997-11-24 -0800, you wrote:
>Hello,Technetters!
>Skipping the horror story,I have a question to printed circuit
>manufacturers:
>How do you ensure the integrity of the plating in small vias?
>We require the manufacturer's cross sections as a proof of test
>for our circuits.Very seldom,they contain small vias.
>But,anyway,the failures found recently in our line are in random places
>on the boards.
>Are there other tests on bare boards which can detect reliability
>problems ?
>
>Thank you
>Gaby
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|