At 09:09 AM 1/27/98 -0500, Sheila Smith wrote:
>Hello,
>
>First, thanks to everyone for the replies to my questions about HASL -- the
>information was very helpful.
>
>Now, does anyone have an experience or data on the effects of radiation on
>silver-filled conductive epoxies? [Radiation exposure as in space
>applications.] The manufacturers of the epoxies say no effects. Thanks in
>advance for your help.
>
>Sheila Smith, Tracor Aerospace
One data point for you Sheila. I was involved with the analysis of a
module which failed during a space mission. The module used a silver
conductive epoxy as the attach media. The silver had migrated from the
silver terminations on a discrete resistor and from the epoxy and caused
circuit failure. Because of the zero-g atmosphere, instead of just getting
migration paths on the surface, the silver grew out in all directions. I
have some very beautiful SEM photographs of silver whiskers, "weeds" and
"shrubs" growing out of component terminations and the epoxy.
---
Gregg Klawson
GTE Government Systems Corp, Taunton, Massachusetts, USA
[log in to unmask], telephone +1.508.880.1822
The views expressed are the author's and do not necessarily reflect the
official position of GTE or any of its subsidiaries.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|