Brian Ellis <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Sun, 29 Aug 2004 10:18:05 +0300
Content-Type:
text/plain
Parts/Attachments:
text/plain (77 lines)
Steve

As far as I'm aware, this clip is in the public domain. I know that
Charles Jennings distributed many 16 mm copies of it. If this is so,
then you don't need my permission. If it is considered copyright, then
you should obtain permission from Sandia (I don't imagine this would be
a problem).

Of course, the tiny image in my download is hardly suitable for
reproduction. I could provide it in a form reproducible on a TV or
computer screen as an SVCD (PAL 480 x 576 pixels 25 fps or NTSC 480 x
480 29.97 fps) or even a DVD (PAL 720 x 576 25 fps or NTSC 720 x 480
29.97 fps). I'd be willing to do this on a non-profit basis, but my
costs (media, conversion and authoring time on specialised equipment,
packing and postage) would have to be covered. (As I'm "retired", living
on a pension, I no longer have a company to sponsor me.) I hope this is
not contravening IPC rules on spamming on the TN.

Brian

Steve Gregory wrote:
> Hi Brian!
>
> What a wonderful video clip! I've been able to repeat the same thing, and
> show that to my operators using a dual-view microscope about the sins of
> hand-cleaning OA residues. They see the same thing as it happens...most are very
> suprised!
>
> May I use this video clip in training documentation? I of course, will
> acknowledge the originator.
>
> Many thanks!
>
> -Steve Gregory-
>
> In  ~1980, Charles Jennings of Sandia National Laboratories,  Albuquerque,
> researched dendrites and published a paper at the 2nd Printed  Circuit
> WorldVonvention in Munich in 1981. He also produced a film  showing
> dendrite growth, which was quite widely distributed. It is possible  that
> some of the younger members of this list have not seen this  classic
> document. You can now download a version of it  at
> http://www.bnellis.com/dendrites/ in the form of a 3 min 50 sec WMV  file
> (~625 kb). This can be played in Windows Media Player.
>
> If there  is sufficient demand, I could put it into other formats/sizes.
>
> The  quality may not be 100% perfect, as I believe the history of my copy
> was  something like 16 mm film > Super 8 film > VHS tape > DV AVI file  >
> WMV file!
>
> Brian
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2