TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Alderete, Michael" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum." <[log in to unmask]>, "Alderete, Michael" <[log in to unmask]>
Date:
Mon, 24 Aug 1998 18:18:08 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (51 lines)
Nick-

Liquidus is about 220 deg C at 90% Sn, 10% Pb, by eyeballing a phase
diagram.
Don't have experience with this solder alloy.

You wrote....
------------------------------

Date:    Mon, 24 Aug 1998 18:18:37 -0400
From:    Nick Nicolaides <[log in to unmask]>
Subject: Solder temperature

My book only goes to 70/30 (tin/lead). need help. Our part supplier is
using
90/10 rather then 63/37. The higher tin causes more oxides creating some
cold solder joints. Supplier has brass base followed by copper flask and
90/10 tin/lead. What is the liquidus temperature of tin/lead of 90/10
and
has anyone had the experience. Also the feet to this part are very small
and
close to the pad. Hard to inspect. We had the supplier go to 63/37 and
had
very little problem. Supplier wants to go back to 90/10. whats the
concensus?

------------------------------

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2