TECHNET Archives

April 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Andre Leclair <[log in to unmask]>
Date:
Tue, 23 Apr 2002 11:09:01 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Andre Leclair <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
We have recently run across a situation which has baffled us.  On the PCB
in question there are 4 Wave soldered PLCC sockets. 1 of these is being
reported as having solder shorts underneath.  On the returned units we x-
rayed the sockets ( can't see under) and found shorts on 1 socket location
only.  The shorts were consistanly on the same pin area for all the sockets
were the shorts were found.  We removed a socket only to find the board
very clean underneath...no shorts..
The socket has a bottom retainer to hold all the pins in place.. This was
pried off and to our surprise there was the short.. inside the connector.
The amount of solder was enough to surround 3 pins in 2 seperate areas.
The hole around the pins in the plastic base is no more then 0.002".

Does any one have any idea how solder could have gotten up inside the
connector ( consistantly in the same location)? Or has any one seen this
before?

We have run this assembly several times in the past with no difficulty.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2