Nee how Don,
The typical preheat sections are tunnel ovens that have a combination of IR
and convection heating.
With ENIG you are trying to solder to nickel which requires considerably more
heat [time and/or temperature] than soldering to copper--not only that, but
in many cases the solder joint is already formed because of HASL.
There are no files attached to your e-mail [IPC strips them off--you can send
them to me directly]--so I cannot comment. However, you may have 'Black Pad'
failures which show up first in SJs that see high temperatures such as would
occur with manual soldering.
I hope this helps.
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|