"Anslow, Phillip" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Anslow, Phillip
Date:
Wed, 15 Jun 2005 14:52:32 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (87 lines)
Hi Steve,
Not my field directly, but while the iron is hot, I wonder how soon it will
be before everybody is pre-baking all the Plastic Encapsulated Devices,
PBGAs etc as well (didn't even mention boards) to make sure all the moisture
is out of them before Pb-Free temperatures hit them? Or am I worrying about
nothing? More energy used - groan.

Thanks by the way for your web page etc.

Regards,
Phil.
My opinion, not my company's.
-----Original Message-----
From: Stephen Gregory [mailto:[log in to unmask]]
Sent: 15 June 2005 14:42
To: [log in to unmask]
Subject: [TN] Baking PLCC-68's...


               *** WARNING ***

This mail has originated outside your organization,
either from an external partner or the Global Internet.
     Keep this in mind if you answer this message.

Just wondering, how many of you have ever baked a
PLCC-68?

We've been raising the awareness level of our stockroom
people about component moisture sensitivity, and we've
got some PLCC-68's that are on a reel and been sitting on
on our stockroom shelf for longer than 168-hours.

Well, we got another reel of the same part number (it's an
Intel i960 PLCC-68) that came to us from Avnet in a vacuum
sealed bag with a level-3 MSL label on it.

I've never baked a PLCC-68...should I bake the reeled parts
that have been sitting on the shelf?

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2