Jim,
You have chemically altered the polymer. It will no longer perform it's designed function.
David A. Douthit
Manager
LoCan LLC
"Marsico, James" wrote:
> Help! Emergency!
>
> We have a completed assembly (top assembly with many boards, hybrids, etc.)
> ready for shipment to our customer (space product). The last operation was
> to ink mark a S/N. The ink is cured at 150 F for 2 hours. The assembly was
> put in an oven at 150 C for two hours. After hours of reviewing all of the
> materials and bill of material, component by component (component data,
> supplier phone calls, etc.), the only item that is not rated for 150 C is
> the polyurethane conformal coating, which turned yellow/brown in color. Can
> anyone explain what actually happened to the coating and if it can be used
> as is?
>
> Thanks,
>
> Jim Marsico
> Senior Engineer
> Production Engineering
> EDO Electronics Systems Group
> [log in to unmask] <mailto:[log in to unmask]>
> 631-595-5879
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|