TECHNET Archives

March 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Tony Lentz <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Tony Lentz <[log in to unmask]>
Date:
Tue, 8 Mar 2016 14:46:32 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (61 lines)
Hello Juliano,

We are a licensed manufacturer of SN100C alloy.  There are many studies and published papers which compare the properties and reliability of SN100C vs. SAC305.  I would be happy to give you the details about it off-line.  

Best regards,

Tony Lentz
FCT Assembly
Field Application
[log in to unmask]
970-566-0360 Mobile



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Datacom - Juliano Ribeiro
Sent: Tuesday, March 8, 2016 4:34 AM
To: [log in to unmask]
Subject: [TN] SAC x SN100C

Hi to all,

 

What are the differences about SAC305/0307 vs SN100C (reliability criteria and process specification)?

I read about SAC0307 and SAC305 and the article shown that SAC0307 is better about Drop Shock but the SAC305 is better about Thermal Cycle. I would like the same comparison about SAC vs SN100C.

 

Thank you a lot

_____________________________

Juliano Bettim Ribeiro

DATACOM 

ENGENHARIA DE PROCESSOS
Rua América Nº 1000 - Eldorado do Sul - RS CEP: 92990-000 
+55 (51) 8446-2135

+55 (51) 3933-3000 

Ramal: 3484
 <mailto:[log in to unmask]> [log in to unmask] 
 <http://www.datacom.ind.br/> www.datacom.ind.br

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2