Earl & Joseph,
I'm not sure what the answer is, but most of the electrolytic Nickel I know of
also contain Phosphorus. Perhaps the answer is in a thicker or electrolytic
Gold.
I'll be interested in the resolution to this one.
Regards,
Les Connally
> From: Earl Moon <[log in to unmask]>, on 7/31/98 8:19 AM:
> Joseph,
>
> I just asked a question concerning phosphorous intermetallic growth as
> in item 16 or so. I was prompted to do so because of a response I
> received some weeks ago concerning the issue you raise.
>
> Again, a major BGA supplier (Motorola) wrote me and confided they found
> the problem associated with their sphere attachment to a substrate using
> the immersion tin and gold processes. To make a long story short,
> someone, at some time dropped a board on the floor detaching BGA devices
> at all their termination points.
>
> My question to industry is what can we do to overcome the phosphorous
> intermetallic and resulting solder joint embrittlement problem? Can we
> go to electroplated nickel in required thicknesses and then deposit
> electroless gold over that?
>
> Earl Moon
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
> text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
> for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|